Grease resistance without PFAS: choosing a label facestock
The EU restriction on PFAS in food-contact packaging applies from August 2026. Six questions on what is limited, whether labels count, and how to prove a fluorine-free face.
The EU restriction on PFAS in food-contact packaging has applied since 12 August 2026, and grease-resistant treatments are squarely in scope. A pressure-sensitive label touching food sits inside that boundary, facestock and adhesive included. Swapping to a fluorine-free face is not a paper change: print settings, die pressure and customer documentation all move with it.
What exactly is limited
Three numbers matter: 25 ppb for a single substance, 250 ppb in total, and 50 ppm for total fluorine. The first two are measured against named compounds, the third by converting all fluorine. Different methods, and sometimes different verdicts on the same sample.

The Commission's March 2026 guidance acknowledged that a harmonised test method is still missing. In practice the inspector looks for self-declaration: a supplier statement, a third-party report and a formulation description. All three, or the file is thin.
Does a label count as food-contact packaging
A label stuck directly onto food counts, no argument. A label on the outer wrapper with film between it and the food depends on whether migration is possible.
Most food labels sit on the outside of a film or carton, which makes the contact indirect. Even then, fluorine from adhesive and facestock has a migration path, and the paperwork request arrives just the same.
A useful order of checking: how many layers sit between label and food, whether those layers block migration, and what compliance position the customer has taken. All three clear, and the label is defensible.
Without a fluorochemical, what blocks the grease
| Route | How it works | Grease hold-out | Trade-off |
|---|---|---|---|
| Dense coating | Close the pores with a tighter coat weight | Moderate, fine for short contact | Surface energy shifts, print needs resetting |
| Heavier paper | Thickness as the barrier | Moderate to good, cost climbs with grammage | Stiffer sheet, harder on curved surfaces |
| Film facestock | PET or PP, no path for oil | Good, oil cannot wick through | Plastic feel, poor story at the recycling end |
This year a European paper mill moved its packaging-paper barrier technology onto an 80 gsm label face, with no intentionally added PFAS, third-party test reports and compliance with FDA and German BfR food-contact requirements. That route suits heavy grease and long contact times.

Press and wipe, and the paper tells you whether it holds grease
What changes on press and die
Start with print. Fluorine-free coatings often carry a higher surface energy than the treatment they replace, so ink spreading changes, solids go blotchy and fine type fills in. Pull a full solid before the run and look at density and edge sharpness.
Then the die. A heavier face needs more pressure to cut clean, and too much pressure marks the liner. The blanket under the die may need a harder grade.
Finally the applicator. A stiffer label springs back faster on a curved bottle, so roller pressure needs resetting.
What to hand the customer
Three documents: a no-added-PFAS declaration from the supplier, a third-party PFAS test report, and a food-contact compliance statement in FDA or BfR terms.
Two details decide whether the file survives: whether the report measured total fluorine or individual substances, and whether the sample was facestock or a finished label. Mismatched scope gets rejected at the border.
How much more it costs
A fluorine-free grease-resistant face usually prices above standard coated paper and close to the fluorinated grade it replaces, depending on grammage and volume. On a small label the gap is often a few cents per thousand.
The real spend is the switch: new samples, re-validated print settings, fresh testing. Small batches cannot absorb that fixed cost, so keep them on the existing face and reserve the fluorine-free grade for export orders.